Liquid Nitro Carborising & Post Oxidation

The process is carried out at 565c. Very hard Compound layer of (Iron nitride) is in the range of 12 micron to 18 micron and diffused layer upto 300 microns. The post oxidation is carried out at 425 c in a different furnace to give non corrosive black surface.